Analysis of Current and Active Flux Variations In Dissimilar A-TIG Welding of Aluminium Grades 5052 and 5083 on Penetration Depth, Microstructure, Hardness Value, Tensile Strength, and Corrosion Rate

Authors

  • Alvalo Toto Wibowo Study Program of Welding and Fabrication Engineering, Surabaya State Shipbuilding Polytechnic, Jalan Teknik Kimia, ITS Campus, Surabaya 6011
  • Moh. Syaiful Amri Study Program of Welding Engineering, Surabaya State Shipbuilding Polytechnic, Jalan Teknik Kimia, ITS Campus, Surabaya 6011
  • Imam Khoirul Rohmat Study Program of Welding and Fabrication Engineering, Surabaya State Shipbuilding Polytechnic, Jalan Teknik Kimia, ITS Campus, Surabaya 6011
  • Rikky Leonard Study Program of Shipbuilding Construction Engineering Technology, Surabaya State Shipbuilding Polytechnic, Jalan Teknik Kimia, ITS Campus, Surabaya 6011
  • Andri Djumiati Study Program of Shipbuilding Engineering, Surabaya State Shipbuilding Polytechnic, Jalan Teknik Kimia, ITS Campus, Surabaya 6011
  • Rocky Andiana Study Program of Welding and Fabrication Engineering, Surabaya State Shipbuilding Polytechnic, Jalan Teknik Kimia, ITS Campus, Surabaya 6011
  • Maulana Basri Nuradan Study Program of Welding Engineering, Surabaya State Shipbuilding Polytechnic, Jalan Teknik Kimia, ITS Campus, Surabaya 6011

DOI:

https://doi.org/10.23960/jemit.534

Keywords:

A-TIG, Active Flux, Aluminium, Current Strength, Dissimilar Welding

Abstract

Dissimilar welding of Aluminum 5052 and Aluminum 5083 is widely used in shipbuilding because of its good strength and corrosion resistance. However, the different properties of the two alloys make it difficult to achieve adequate weld penetration using conventional TIG welding. Therefore, the Activated Tungsten Inert Gas (A-TIG) process with TiO2 and ZnO active fluxes was used to improve penetration through an arc-constriction mechanism. This study investigated the effects of welding current (190, 210, and 230 A) and active flux type on penetration depth, microstructure, hardness, tensile strength, and corrosion rate. The results showed that the deepest penetration was achieved using ZnO (7.21 mm), followed by TiO2 (7.02 mm), while welding without flux yielded only 4.89 mm. The weld microstructure was dominated by the alpha-Al phase, with finer and more evenly distributed Mg2Si intermetallic particles. The highest weld metal hardness was obtained with TiO2 (72.6 HVN), while ZnO provided the highest tensile strength (196.54 MPa) and the lowest corrosion rate (0.133 mmpy). Overall, the A-TIG process improved the quality of dissimilar welding between Aluminum 5052 and Aluminum 5083, with ZnO active flux providing the best overall test results.

Downloads

Download data is not yet available.

References

American Society of Mechanical Engineers. (2019). 2019 ASME boiler and pressure vessel code: Section II—Materials, Part B—Nonferrous material specifications. ASME.

ASTM International. (2004). Standard practice for laboratory immersion corrosion testing of metals (ASTM Standard No. G31-72(2004)). https://store.astm.org/g0031-72r04.html

ASTM International. (2023). Standard test methods for Vickers hardness and Knoop hardness of metallic materials (ASTM Standard No. E92-23). https://store.astm.org/e0092-23.html

ASTM International. (2025). Standard test methods for tension testing of metallic materials (ASTM Standard No. E8/E8M-25). https://store.astm.org/standards/e8_e8m

Bahariawan, A. F. (2021). Analisis hubungan variasi preheat dengan metode single dan double side arc welding pada material aluminium 5052 terhadap struktur mikro dan sifat mekanik [Undergraduate thesis, Politeknik Perkapalan Negeri Surabaya].

Bahri, G. B. Q. (2022). Analisis pengaruh active flux ZnO dan SiO2 dan kuat arus pada pengelasan A-TIG aluminium 5083 terhadap kedalaman penetrasi, nilai kekerasan, dan metallography [Undergraduate thesis; institution to be confirmed].

Firmansyah, F. (2021). Pengaruh active flux (TiO2 dan SiO2) dan kuat arus pada pengelasan A-TIG dissimilar material terhadap kedalaman penetrasi, struktur mikro, nilai kekerasan, dan ferrite content [Undergraduate thesis, Politeknik Perkapalan Negeri Surabaya].

Fontana, M. G., & Greene, N. D. (2018). Corrosion engineering. McGraw-Hill.

Ilmihadiyat, F. (2025). Analisis pengaruh active flux TiO2, SiO2, dan kuat arus pada pengelasan A-TIG pada aluminium 5052 terhadap kedalaman penetrasi, struktur mikro, nilai kekerasan, dan kekuatan tarik [Undergraduate thesis; institution to be confirmed].

Jawwad, M. I. Al. (2022). Analisis pengaruh active flux (MgCl2 dan TiO) dan kuat arus pada pengelasan A-TIG aluminium 5083 terhadap nilai kekerasan dan metalografi [Undergraduate thesis, Politeknik Perkapalan Negeri Surabaya].

Kim, M., Perez-Andrade, L., Brewer, L. N., & Kubacki, G. W. (2024). Effect of microstructure on corrosion behavior of cold sprayed aluminum alloy 5083. Corrosion and Materials Degradation, 5(1), 27–51. https://doi.org/10.3390/cmd5010002

Munir, M. M., Wahyudi, M. T., Kurniyanto, H. B., & Anggara, D. (2019). Modul praktik DT NDT [Practical module; publisher or institution to be confirmed].

Nugroho, W. Y. (2023). Studi pengaruh TiO2-SiO2 sebagai active flux terhadap penetrasi pengelasan A-TIG pada material aluminium seri 5083-H116. Jurnal Inovasi Teknologi Manufaktur, Energi, dan Otomotif, 1(2), 84–94. https://doi.org/10.57203/jinggo.v1i2.2023.84-94

Purnama, R., Wa'adulloh, M., Hamid, A., & Sutrisno. (2024). Analisis komparatif laju korosi pada material aluminium 5083 dan 5052 dengan menggunakan media air laut sebagai aplikasi bahan lambung kapal [Undergraduate thesis; institution to be confirmed].

Ramadani, D. T. (2023). Analisis active flux MgO dan CaF2 dan kuat arus pada pengelasan A-TIG aluminium 6061 terhadap kedalaman penetrasi, nilai kekerasan, struktur mikro, dan laju korosi [Undergraduate thesis, Politeknik Perkapalan Negeri Surabaya].

Ridho, A. F., & Rokhim, I. N. (2023). Analisis teknis dan ekonomis korosi perbandingan ASTM A36 dan aluminium 5083 untuk pelat kapal. JUSTI (Jurnal Sistem dan Teknik Industri), 4(3), 303–311.

Rizki, A. M. (2018). Analisis pengaruh variasi elektroda pada pengelasan aluminium 5083 dengan 6061 terhadap sifat mekanik, struktur mikro, dan prediksi korosi [Undergraduate thesis, Institut Teknologi Sepuluh Nopember].

Rohmat, I. K., Ramadhan, M. I., & Anggara, D. (2022). Pengaruh jenis activated flux dan variasi kuat arus pada pengelasan A-TIG dissimilar material terhadap kedalaman penetrasi, kekerasan, struktur mikro, dan laju korosi. JTT (Jurnal Teknologi Terapan), 8(2), 131–138.

Rupajati, P., & Anggoro, I. B. (2020). Karakteristik proses pengelasan TIG pada aluminium 5052 dan aluminium 6061 terhadap sifat mekanis dan struktur mikro untuk aplikasi rangka pelindung (roll cage) pada mobil balap rally [Publication type and institution to be confirmed].

Tajul Arifin, M. H. (2024). Analisis active flux component dan TIG welding method dengan material stainless steel 304 terhadap kedalaman penetrasi, kekuatan tarik, dan nilai kekerasan. INOVTEK Polbeng, 14(2), 208–215.

Tarmizi, T., Sianturi, K. D., & Irfan, I. (2020). Effect of current on mechanical properties and microstructure of aluminum 6061 with gas tungsten arc welding process. Kapal: Jurnal Ilmu Pengetahuan dan Teknologi Kelautan, 17(3), 107–113. https://doi.org/10.14710/kapal.v17i3.30054

Wiryolukito, S., & Wijaya, J. P. (2020). Result analysis of friction stir welding of aluminum 5083-H112 using taper threaded cylinder pin with variation in rotational and translational speed. AIP Conference Proceedings, 2262(1), Article 070003. https://doi.org/10.1063/5.0016148

Downloads

Published

2026-11-25

How to Cite

Wibowo, A. T., Amri, M. S. ., Rohmat, I. K. ., Leonard, R. ., Djumiati, A. ., Andiana, R. ., & Nuradan, M. B. . (2026). Analysis of Current and Active Flux Variations In Dissimilar A-TIG Welding of Aluminium Grades 5052 and 5083 on Penetration Depth, Microstructure, Hardness Value, Tensile Strength, and Corrosion Rate. Journal of Energy, Material, and Instrumentation Technology, 7(4), 297–305. https://doi.org/10.23960/jemit.534